selective negative resist stripper
Javier Crespo
Dear All, Could anyone tell me how could I remove negative photoresist from a silicon wafer without affecting metal layer (Ni or AlSi)? I know that the piranha etching etches the resist in a higher rate than the metal, but I don't know in which percentage. Best regards,