We have got some surplus good quality 4inch/100mm SOI wafers for re-sale.
You can find their specs below. Please let us know immediately if you are
interested in buying these in full or part. We will offer you the best
price, much better than what we paid for them from the commercial wafer
vendor. If you are interested, the wafer history is also available.

Regards,

Napp Jones


* Read -- um => micron
--------------------------------------------------------------------------------
-------------------------
1. 1.5 um SOI wafers (SOITEC) - suitable for IC & MEMS
--------------------------------------------------------------------------------
-------------------------

* Available Quantity - 12x pcs

* Orientation - (100)

* Device Silicon Layer - Thickness/Type/Resistivity:
  1.5 um/P-type (B)/14-18 ohm-cm

* Oxide (BOX) Layer Thickness - 1.0 um

* Handle Silicon Layer - Thickness/Type/Resistivity:
  400 um/N-type(Ph)/0.3-1.2 ohm-cm

* Double-side Polished (DSP): Yes

------------------------------------------------------------------------------
2.  3 um SOI wafer - suitable for MEMS
-----------------------------------------------------------------------------

* Available Quantity - 1x pcs

* Orientation - (100)

* Device Silicon Layer - Thickness/Type/Resistivity:
  3.0 um/P-Type(B)/4-6 ohm-cm

* Oxide (BOX) Layer Thickness - 1.0 um

* Handle Silicon Layer - Thickness/Type/Resistivity:
  ~500.0 um/P-type(B)/na

* Double-side Polished (DSP): No

--------------------------------------------------------------------------------
-----------
3. 25 um SOI wafer (Ultrasil) - suitable for MEMS
--------------------------------------------------------------------------------
-----------

* Available Quantity - 1x pcs

* Orientation - (100)

* Device Silicon Layer - Thickness/Type/Resistivity:
  25 um +|- 0.5 um/P-Type(B)/0.02-0.05 ohm-cm

* Oxide (BOX) Layer Thickness - 3.0 um

* Handle Silicon Layer - Thickness/Type/Resistivity:
  465.0 um +|- 5.0 um/P-Type(B)/0.01-0.02 ohm-cm

* Double-side Polished (DSP): Yes

--------------------------------------------------------------------------------
--------------
4. 27.5 um SOI wafer (Ultrasil) - suitable for MEMS
--------------------------------------------------------------------------------
---------------

* Available Quantity - 1x pcs

* Orientation - (100)

* Device Silicon Layer - Thickness/Type/Resistivity:
  25um +|- 0.5 um, P-Type(B)- 2.0um, N-Type(As) - 0.5 um, P-Type(B)/<0.05
ohm-cm

* Oxide (BOX) Layer Thickness - 3.0 um

* Handle Silicon Layer - Thickness/Type/Resistivity:
  465.0 um +|- 5.0 um/P-Type(B)/0.01-0.02 ohm-cm

* Double-side Polished (DSP): Yes

--------------------------------------------------------------------------------
--------------------------
5. 47 um +/- 3 um SOI wafers (Ultrasil) - suitable for MEMS
--------------------------------------------------------------------------------
---------------------------

* Available Quantity - 2x pcs

* Orientation - (100)

* Device Silicon Layer - Thickness/Type/Resistivity:
  47.0 um +|- 3.0 um/P-Type(B)/<0.05 ohm-cm

* Oxide (BOX) Layer Thickness: 2.0 um

* Handle Silicon Layer - Thickness/Type/Resistivity:
  300.0 um/P-Type(B)/<0.05 ohm-cm

* Double-side Polished (DSP): Yes

------------------------------------------------------------------------------
reply
Jobs
Resumes
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
Brewer Science
MEMS Industry Group
Coventor